Polarization SiliconeOxide Subhajjit ForceVolume LMF ScanningTunnelingMicroscopy Polyethylene Lanthanum_aluminate Aluminium_Oxide LiquidImaging Dr.JurekSadowski Microchannel Styrene chemical_compound Implant Barium_titanate HumanHair Magnets doped Tapping gallium_nitride Led Scratch Wonseok Gallium_Arsenide Hexacontane FuelCell hard_disk FM_SKPM temperature_control Crystal PolymerBlend SrO thermoplastic_elastomers HfO2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V