Ecoli ContactModeDot Polyaniline Gallium_Arsenide PMNPT Fujian SoftSample Phase PinpointPFM GlassTemperature Forevision domain_switching LiIonBattery DentalProsthesis DomainSwitching Co/Cr/Pt ScanningSpreadingResistanceMicroscopy PVAC graphene_hybrid INSPParis Korea PhaseTransition hard_disk_media MagneticPhase AnodizedAluminumOxide KevlarFiber Annealing CeramicCapacitor Hole fluoroalkane electrospinning University_of_Regensburg NiFe Ito Insulator
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512