Treatment biocompatible Molybdenum CalciumHydroxyapatite OpticalModulator fluorocarbon blended polymers CeramicCapacitor Tungsten_disulfide LFM Dr.JurekSadowski Modulus NiFe Display Electrical&Electronics Glass piezoelectric force microscopy Vacuum CBD Hexylthiophene WWafer Fujian MultiferroicMaterials Array PhaseChange EFMAmplitude FloppyDisk heterojunctions ElectrostaticForceMicroscopy YszSubstrate MolybdenumDisulfide Piezoelectric HDD plastic Chromium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Galfenol (Alloy of iron and gallium)
Scanning Conditions
- System: XE15
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=70kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- MFM Lift height: 50nm