BreastCancerCell Pyroelectric UnivCollegeLondon Spain LightEmiting Bmp thermal_conductivity BismuthVanadate Wonseok Spincast Strontium rubber NCM Sapphire GlassTemp PolycrystallineFerroelectricBCZT BiFeO3 Roughness Blood Copolymer Dental SAM LateralForce Current AmplitudeModulation CVD Non-ContactMode HighResolution suspended_graphene GaP SFAs Electrical&Electronics Fet Piranha OpticalElement
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian