LDPE small_scan CVD MechanicalProperty Worcester_Polytechnic_Institute FFM Non-ContactMode Spincast PrCurve PhaseImaging Lattice Global_Comm ItoGlass Bismuth Stiffness molecular_beam RedBloodCell UnivMaryland Chemical_Vapor_Deposition Mechanical Sperm Zagreb cannabidiol CompactDisk graphene_hybrid AdhesionEnergy Molybdenum Tin disulfide DNA ThermalConductivity HardDiskMedia HiVacuum Regensburg DiffractiveOpticalElements BTO
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene
Scanning Conditions
- System: XE7
- Scan Mode: Conductive AFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256