Acoustic Enclosures
AFMs measure properties at the nanometer scale, so every small factor can have a large effect on accuracy. That’s why Park has developed some of the best acoustic enclosures on the market, isolating the instrument from noise and helping to make Park AFMs the world’s most accurate.
Acoustic Enclosure 202
Specifications :
Environmentally sealed acoustic enclosure to block external acousticand light noise
Dimensions: 820 × 920 × 1,360 mm (outer dimension, W x D x H)
Weight: 350 kg
* For NX20
Acoustic Enclosure 203
The Acoustic Enclosure 203 may come standard with the NX10, but its acoustic isolation performance is anything but. Active vibration isolation, and an ergonomic design make it one of the most effective and easy to use acoustic enclosures on the market.
Specifications :
Includes an active vibration isolation system for extreme vibration isolationErgonomic design for convenient access to the instrument
Dimensions: 700 × 900 × 1,300 mm for NX10
Weight: 300kg for NX10 Standard AE
Active Temperature Control for Acoustic Enclosure 203
For those that need precise temperature control and incredible acoustic isolation for their NX AFM. This enclosure maintains a thermally stable environment within 10 minutes of activation.
Specifications :
- Innovative control design brings the enclosure quickly to its temperature equilibrium- Temperature variability of less than 0.1°C within 10 minutes of closing the door
Acoustic Enclosure 101
Our easiest to handle AE, the Acoustic Enclosure 101 weighs just 40 kg, while still effectively isolating your AFM from unwanted noise.
Specifications :
Environmentally sealed acoustic enclosure to block external acoustic and light noiseErgonomic design for user convenience
Dimension: 510 × 715 × 630 mm (outer dimension, W x D x H)
Weight: 40 kg
Acoustic Enclosure 201
Designed exclusively for the XE series, the Acoustic Enclosure 201 isolates the XE system from external acoustic and light noise for exact precision. The unit can also be equipped with an active vibration isolation table for even better performance.
Specifications :
Granite table provides increased vibration isolationBest solution for sub-nanometer scale high resolution imaging
Ergonomic design for a convenient access to the instrument
Dimension: 820 × 920 × 1,345 mm (outer dimension, W x D x H)
* For XE7 / XE15 only
Acoustic Enclosure 204
Specifications :
Best solution for high resolution in-liquid imagingErgonomic design for a convenient access to the instrument
Dimension: 880 × 1,000 × 1,500 mm (outer dimension, W x D x H)
Weight: 385 kg
* For NX12
Acoustic Enclosure 401
Specifications :
Acoustic enclosure designed for industrial environmentDimension: 880 × 980 × 1,460 mm (outer dimension, W x D x H)
Weight: 595 kg