heterojunctions GlassTemp Gold epitaxy AlkaneFilm Microchannel FastScan Adhesive PetruPoni Calcium fluoroalkane UnivMaryland biocompatible PtfeFilter 2-vinylpyridine PolyimideFilm Biology TungstenThinFilmDeposition nanobar LiftHeight NTU molecule DIWafer TiO2 Pinpoint PFM phase_change BFO LiquidCell Floppy Reduction Polyvinylidene_fluoride BTO TemperatureControllerAFM AM-KPFM LightEmiting
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer thin film
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512