nanomechanical CompactDisk mono_layer single_layer Pinpoint FrictionForce fifber ScanningKelvinProbeMicroscopy Piezoelectric Piranha suspended_graphene HanyangUniv Butterfly Vortex FrequencyModulation BismuthVanadate Iron FM_SKPM Inorganic Vac C36H74 DentalProsthesis SrO sputter Blood organic_polymer CeNSE_IISc Hafnia Nanostructure P3HT Foil IRDetector Cobalt SKPM Calcite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V