single_layer Change #EC Ram SSRM aluminum_nitride AdhesionEnergy Hole fluorocarbon SKPM LifeScience CuFoil silicon_carbide FloppyDisk Conducting MLCC Sic LateralPFM Dr.JurekSadowski LightEmiting SPMLabs NTU Vortex TappingMode Grain Chloroform Growth PMNPT Mechanical&nanotechnology SingleCrystal EPFL Calcite Ferrite DeflectionOptics LithiumNiobate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Diffractive Optical Elements
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 40μm×40μm, 5μm×5μm
- Scan Rate: 0.3Hz, 0.4Hz
- Pixel: 512×256, 512×256