Growing temperature_control Nanofiber SurfaceChange Optoelectonics Molybdenum_disulfide Patterns Optical Cancer Polyimide Co/Cr/Pt cannabis SolarCell PyroelectricDetector H-BN FAFailureAnlaysis MBE Conductive AFM Step MeltingPoint Mapping Ni-FeAlloy PolymerBlend Wonseok IIT-chennai Aggregated_molecules LiBattery TipBiasMode ThermalProperties Conductivity BloodCell BoronNitride piezoelectric force microscopy VinylAlcohol Device
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BiVO4 on treated YSZ substrate
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.36Hz
- Pixel: 256×256