GranadaUniv PolymerPatterns temperature controller AFM Sidewall FastScan Gong atomic_steps atomic_layer Polyurethane TriGlycineSulphate Polyvinylidene_fluoride Film solar_cell Copolymer FrequencyModulation DiffractiveOpticalElements thermal_property Ananth Magnetic Force Microscopy LMF Terrace LifeScience multi_layer ContactModeDot AlkaneFilm Conductance Conductivity IcelandSpar Polyimide AnodizedAluminumOxide MLCC Granada ReflexLens LiNbO3 IVSpectroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PMN-PT single crystal
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: NSC36A Ti-Pt (k=1N/m, f=90kHz)
- Scan Size: 8μm×8μm
- Scan Rate: 0.5Hz
- Pixel: 512×256