Biology MagneticPhase DentalProsthesis membrane TipBiasMode Techcomp LateralForceMicroscopy Ca10(PO4)6(OH)2 LiIonBattery contact Organic Phosphide Vac Wonseok F14H20 OpticalWaveguides LeakageCurrent semifluorinated_alkanes EPFL ForceDistanceSpectroscopy Current Nanopattern Electrical&Electronics Wafer Chrome 2dMaterials lithography Corrosion bias_mode UnivMaryland MLCC CopperFoil fluorocarbon Calcium Memory
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Diffractive Optical Elements
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 40μm×40μm, 5μm×5μm
- Scan Rate: 0.3Hz, 0.4Hz
- Pixel: 512×256, 512×256