CrossSection H-BN Hexacontane Molybdenum_disulfide Piezo UnivCollegeLondon KevlarFiber PinpointNanomechanicalMode Plug OpticalElement polyvinyl acetate HardDisk LDPE mechanical_property DNAProtein Thermal Barium_titanate Bismuth ring shape GaP hydrocarbon SICM Yeditepe_University Microchannel CopperFoil Copolymer CompactDisk PMNPT SrO Protein PhaseChange Ucl Electrode suspended_graphene BariumTitanate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene
Scanning Conditions
- System: XE7
- Scan Mode: Conductive AFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256