OpticalWaveguides Melt Led LogAmplifier Tin sulfide C_AFM ImideMonomer P3HT CancerCell Hydroxyapatite Glass PolymerPatterns Litho margarine Patterns HardDiskMedia Techcomp Optoelectonics KelvinProbeForceMicroscopy Hexylthiophene Lift Hafnium_dioxide Chemical_Vapor_Deposition HexacontaneFilm Granada alkanes Formamidinium_lead_iodide MechanicalProperties Co/Cr/Pt cannabinoid BaTiO3 GaP Polymer HafniumDioxide Protein
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V