Sio2 FM_SKPM Monisha PS_LDPE HDD Galfenol Annealing Vac Vacuum Pzt neodymium_magnets ContactMode polymeric_arrays LiquidCrystal HexagonalBoronNitride SSRM LDPE HafniumDioxide Forevision CeramicCapacitor Friction SoftSample thermal_conductivity DentalProsthesis BaTiO3 biocompatible FloppyDisk TungstenDeposition Laser Step AdhesionForce Copper MagneticArray fluorocarbon YszSubstrate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512