BreastCancerCell Polyethylene Ferrite Foil strontiu_titanate Chemical Vapor Deposition Sic TappingMode Aluminum Alkane PECurve Sperm IVSpectroscopy NusEce Barium_titanate Non-ContactMode Varistor CuFoil Conducting KelvinProbeForceMicroscopy Phenanthrene ReflexLens PiezoelectricForceMicroscopy Ceramics Cell BiasMode TyphimuriumBiofilm OxideLayer Ptfe ScanningSpreadingResistanceMicroscopy temp hard_disk_media CBD Perovskite PolyStylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Galfenol (Alloy of iron and gallium)
Scanning Conditions
- System: XE15
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=70kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- MFM Lift height: 50nm