semifluorinated alkane OpticalModulator Piezoelectric Bmp MetalCompound LMF ReflexLens Device OrganicSemiconductor PolycrystallineFerroelectricBCZT molecular_beam pulsed_laser_deposition Ceramic Chemical Vapor Deposition EFMAmplitude Steps Pore Conducting Cell Metal OpticalElement CarbonNanotube ThermalConductivity Multiferroic_materials BloodCell Vac Moire LeakageCurrent Film AtomicLayer neodymium_magnets Spincast NCM\ Chrome MoirePattern
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- TCS: Temperature control stage type2