pinpoint mode Calcium Ito Ram ShenYang Carbon Platinum Gallium Conducting Collagen Self-assembledMonolayer atomic_layer Magnetic AlkaneFilm FailureAnalysis Temperature GlassTemperature dielectric trench Fe_film cannabidiol Epoxy OrganicSemiconductor bias_mode Graphite CopperFoil mechanical_property thermal_conductivity FM_SKPM Molybdenum_disulfide PhaseChange MembraneFilter Deposition BariumTitanate Cobalt self_assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semiconductor device, W-plug
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: ElectriMulti75-G (k=3N/m, f=75kHz)
- Scan Size: 2μm×1μm
- Scan Rate: 0.3Hz
- Pixel: 512×256
- Sample bias: +1V