BiasMode medical Hair PinpointNanomechanicalMode DOE Mobile phase_change NUSNNI Cross-section DentalProsthesis bias_mode CalciumHydroxyapatite PhaseChange FuelCell PhaseTransition mfm_amplitude heterojunctions TemperatureControlledAFM Scanning_Thermal_Microscopy STM SiliconOxide Sulfur UnivOfMaryland PolyStylene Polytetrafluoroethylene MfmAmplitude PhthalocyaninePraseodymium ito_film ScanningIon-ConductanceMicroscopy molecular_self_assembly HydroGel cross section Electrical&Electronics OpticalWaveguides DeflectionOptics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single layer Graphene film on Cu foil
Scanning Conditions
- System: XE7
- Scan Mode: FM-KPFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256