Using a cantilever as a nanometer scale contact, IV spectroscopy provides a plot of the current (I) as a function of the tip bias voltage (V) applied to a sample. In order to investigate the electrical properties of the sample surface, IV spectroscopy is measured on the selected sample area after taking a sample image.