oxide_layer Pinpoint PFM IMT_Bucharest HanyangUniv Heat Temasek_Lab LiquidCell PDMS Collagen bias_mode AdhesionEnergy TransitionMetal alkanes HDD VinylAlcohol University_of_Regensburg Patterns PMNPT CalciumHydroxide Composition electrospinning FrictionForce Electical&Electronics PtfeFilter FuelCell MagneticPhase MLCC C60H122 ring shape ThermalProperties piezoelectric force microscopy membrane Nickel Flake CHRYSALIS_INC
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm, 5μm×5μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 4096×2048, 512×512