LogAmplifier Monisha Corrosion TiO2 MBE Inorganic_Compound DentalProsthesis Melt 2d_materials plastic Perovskite Subhajjit Anneal semifluorinated_alkanes AM_KPFM HOPG Temasek_Lab FFM flakes TCS Liquid FloppyDisk LateralPFM InLiquid Worcester_Polytechnic_Institute temp Cancer neodymium_magnets Dopped Composition 2-vinylpyridine Hafnium_dioxide Fiber Magnetostrictive NUS
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Styrene beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512