Implant PUR FAPbI3 Polydimethylsiloxane SiWafer thermoplastic_elastomers Plug Switching 2d_materials Cancer multi_layer FFM cooling Filter Display InsulatorFilm GaN doped SAM Growing PolyStylene Magnetic Force Microscopy Lanthanum_aluminate Growth Iron Kevlar SKPM SPMLabs Pore EFMAmplitude Molybdenum_disulfide Ecoli HOPG Mosfet SICM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on STO(110)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.62Hz
- Pixel: 512×512