For optimal performance with our AFM systems please request a quote from Park Systems. Mounted cantilevers are additionally tested. All probes that are not listed here from Adama Innovations, Applied Nano Structures, Inc, BudgetSensors, MikroMasch, Nanosensors™, Nanotools GmbH, Nanoworld AG, NuNano, Olympus Corp., are possible to order from our probe store. Probes from other manufacturers also can be possible to order upon request for quotation. The performance of probes ordered from other sources are not guaranteed.

Probe Force Constant (N/m) Frequency (kHz ) Manufacture Short Description Quote
PPP-CONTSCR 0.2 25 Nanosensors ▪ Contact cantilever
▪ Backside reflex coating (Al)
Request for Quote

The NANOSENSORS™ PPP-CONTSCR is an alternative cantilever type for contact mode applications. The length of cantilever is reduced with respect to the preferred contact mode type enabling easier exchange with non-contact mode probes for some AFM instruments. Additionally, this probe type allows the application for lateral or friction force mode.

Technical Data Nominal Value Specified Range
Thickness /µm 1 0.1-2.0
Mean Width /µm 48 40 - 55
Length /µm 225 215 - 235
Force Constant /(N/m) 0.2 0.01 - 1.87
Resonance Frequency /kHz 23 1 - 57
NSC36/Al BS 1
2
0.6
90
130
65
Mikromasch ▪ Contact cantilever
▪ Backside reflex coating (Al)
▪ 3 cantilevers on a chip
Request for Quote
.
NSC36,
Cantilevers
Resonance Frequency, kHz Force Constant, N/m Length
l ± 5,
µm
Width
w ± 3,
µm
Thickness
t ± 0.5,
µm
min typ max min typ max
A 30 90 160 0.1 1 4.6 110 32.5 1.0
B 45 130 240 0.2 2 9 90 32.5 1.0
C 25 65 115 0.06 0.6 2.7 130 32.5 1.0
PNP-DB 0.48
0.03
67
17
Nanoworld ▪ Contact cantilever made of silicon nitride
▪ Backside reflective coating (Au)
▪ 2 cantilevers on a chip
Request for Quote
Cantilever Data Cant. 1 Cant. 2
Thickness 0.5 µm 0.5 µm
Mean Width 40 µm 40 µm
Length 100 µm 200 µm
Force Constant 0.48 N/m 0.06 N/m
Resonance Frequency 67 kHz 17 kHz
NSC36/HARD/AI BS 1
2
0.6
90
130
65
Mikromasch ▪ Contact cantilever
▪ Backside reflective coating (Al)
▪ 3 cantilevers on a chip
▪ Hard Diamond-Like-Carbon coated tip
Request for Quote
NSC36,
Cantilevers
Resonance Frequency, kHz Force Constant, N/m Length
l ± 5,
µm
Width
w ± 3,
µm
Thickness
t ± 0.5,
µm
min typ max min typ max
A 30 90 160 0.1 1 4.6 110 32.5 1.0
B 45 130 240 0.2 2 9 90 32.5 1.0
C 25 65 115 0.06 0.6 2.7 130 32.5 1.0
PNP-DB 0.48
0.03
67
17
Nanoworld ▪ Contact cantilever made of silicon nitride
▪ Backside reflective coating (Au)
▪ 2 cantilevers on a chip
Request for Quote
Cantilever Data Cant. 1 Cant. 2
Thickness 0.5 µm 0.5 µm
Mean Width 40 µm 40 µm
Length 100 µm 200 µm
Force Constant 0.48 N/m 0.06 N/m
Resonance Frequency 67 kHz 17 kHz
PNP-TR 0.32
0.08
67
17
Nanoworld ▪ Contact cantilever made of silicon nitride
▪ Backside reflective coating (Au)
▪ 2 triangular cantilevers on a chip
Request for Quote
Cantilever Data Cant. 1 Cant. 2
Thickness 0.5 µm 0.5 µm
Mean Width 13.5 µm 28 µm
Length 100 µm 200 µm
Force Constant 0.32 N/m 0.08 N/m
Resonance Frequency 67 kHz 17 kHz
PPP-LFMR 0.2 23 Nanosensors ▪ Contact cantilever with high sensitivity for lateral/frictional force measurement
▪ Backside reflective coating (Al)
Request for Quote
Cantilever Data Nominal Value Specified Range
Thickness /µm 1 0.1 - 2.0
Mean Width /µm 48 40 - 55
Length / µm 225 215 - 235
Force Constant /(N/m) 0.2 0.01 - 1.87
Resonance Frequency /kHz 23 1 - 57

Experience our product's high-quality, precise, and long life backed by our worldwide service network. We are strongly committed to maintaining the quality of our products, making us a trustworthy choice for all your repair and maintenance needs.

We await your inquiry and will arrange for you to speak with a specialist today to explore tailored solutions for your research needs. Please fill out the form now, and we will promptly get in touch with you.

Don't miss out on new product announcements, the latest tech insights, special events, and more. Subscribe now to receive regular updates straight to your inbox!