Alloy ReflexLens FM-KPFM Chungnam_National_University PatternedSapphireSubstrat Anneal DeflectionOptics PinpointNanomechanicalMode LifeScience MagneticArray IRDetector Chemical Vapor Deposition Polypropylene Hafnia CHRYSALIS_INC ScanningIon-ConductanceMicroscopy molecules Perovskite PolymerBlend LDPE CopperFoil polymeric_arrays Titanate ThinFilm thermal_conductivity Magnets strontiu_titanate PS_PVAC SrTiO3 HighAspect PhaseTransition Ni-FeAlloy Piezo GaN Hair
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256