University_of_Regensburg Korea Electronics HDD ItoGlass AM_KPFM Polyvinylidene_fluoride Polyaniline PUR OpticalWaveguides ito_film silicon_oxide HumanHair PolyStylene ThinFilm ScanningKelvinProbeMicroscopy DeflectionOptics Tapping CVD TransitionMetal Epoxy Composition Optoelectonics Co/Cr/Pt Titanate Carbon FailureAnlaysis Thermoplastic_polyurethane Sadowski biocompatible FailureAnalysis PMNPT H-BN IcelandSpar Polarization
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256