ForceMapping Pinpoint PFM Tin disulfide AdhesionForce Nanopattern Optical ConductingPolymer Hexatriacontane HACrystal Mobile TemperatureControllerStage Morphology MultiLayerCeramicCapacitor HexacontaneFilm MLCC TemperatureControl margarine CeramicCapacitor PyroelectricDetector Hafnium_dioxide GaP cannabinoid 2-vinylpyridine DeflectionOptics Conductive AFM WPlug MESA structure STM INSP TriGlycineSulphate ForceDistanceSpectroscopy ReflexLens SKPM Corrosion ferromagnetic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NCA of Li-ion battery (2/2)
Scanning Conditions
- System : NX-Hivac
- Sample bias: 1 V
- Scan Mode: SSRM
- Scan Rate : 0.25Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : AD-40-AS (k=40N/m, f=200kHz)