Hydroxyapatite AAO LiftMode Fluoride LithiumNiobate AnodizedAluminumOxide Photovoltaics SFAs Organic Dental TemperatureControlledAFM Chungnam_National_University Gold Workfunction VerticalPFM PetruPoni non_contact graphene_hybrid Magnets Jason atomic_layer Ni-FeAlloy aluminum_nitride nanobar Fet OpticalWaveguide Hexacontane C_AFM Nanostructure Styrene Oxide ScanningKelvinProbeMicroscopy Piezoresponse self_healing Indent
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Triple-cation perovskite
Scanning Conditions
- System : NX10
- Sample bias: 0 V, 0.5 V
- Scan Mode: C-AFM with PCM toolkit
- Scan Rate : 0.25 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : ANSCM-PC (k=0.2N/m, f=12kHz)