IISCBangalore Hole Pinpoint PFM PolycrystallineFerroelectricBCZT GlassTemp Magnetic chemical_compound SRAM LiftMode solar_cell Pores cross section Chrome light_emitting Alloy Growing Bismuth Patterns ElectroChemical RedBloodCell Sulfur Polarization LiIonBattery SiliconCrystal LateralForce PS_PVAC LowDensityPolyethylene gallium_nitride sputter NCM\ Magnetostrictive light_emission LiquidCrystal ThermalConductivity ImideMonomer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian