Piranha BariumTitanate AM_KPFM doped AM-KPFM Oxidation Magnetic Sio2 UnivMaryland Force-distance AdhesionForce BreastCancerCell atomic_layer ImideMonomer Granada block_copolymer Formamidinium_lead_iodide LightEmiting MagneticPhase AnodizedAluminumOxide TemperatureControllerAFM Hysteresys SiliconeOxide SKKU PiezoelectricForceMicroscopy LateralForce LateralPFM YttriaStabilizedZirconia CP-AFM heterojunctions molecules CeramicCapacitor GranadaUniv conductive SingleCrystal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256