SiWafer atomic_layer PolymerPatterns single_layer WPlug YttriaStabilizedZirconia Bacterium semifluorinated alkane lift_mode Array Mosfet OpticalWaveguide alkanes SelfAssembly GalliumPhosphide DomainSwitching SicMosfet Silver molecules FuelCell PyroelectricDetector contact LogAmplifier EPFL bias_mode GaP Implant LiquidCrystal Conductivity Flake Force-distance Piranha SoftSample NanoLithography TriGlycineSulphate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512