DentalProsthesis MetalCompound Defects Yeditepe_University Yeditepe vertical_PFM FastScan Barium_titanate Pinpoint PFM Boundary RedBloodCell Indium_tin_oxide SiliconOxide BiasMode ScanningTunnelingMicroscopy amplitude_modulation AtomicLayer Perovskite Ceramic Worcester_Polytechnic_Institute SiliconCrystal atomic_steps Composition LiIonBattery Hafnium_dioxide rubber Temperature pinpoint mode Mechinical UTEM Hysteresys ConductiveAFM Polyvinylidene_fluoride Gold MultiLayerCeramicCapacitor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe Thin Films
MFM images of Fe thin films (80 nm) epitaxied on GaAs(001) and then implanted with N-atoms. Images reveal weak stripe domains at magnetic remanence.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm