NUS_Physics Switching Alloy Conductivity 3-hexylthiophene Polyvinylidene_fluoride #EC Leakage INSPParis pulsed_laser_deposition HighResolution temperature controller AFM Piranha LDPE HanyangUniv Annealed Crystal Indent Floppy BariumTitanate Conduct Varistor Adhesive dielectric trench PinpointPFM Oxidation Optoelectonics MeltingPoint LateralForceMicroscopy domain_switching I-VSpectroscopy KevlarFiber ScanningIon-ConductanceMicroscopy Temasek_Lab KelvinProbeForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Mechanical Exfoliated WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.4Hz
- Pixel: 512 × 256