graphene_hybrid Hysteresys IndiumTinOxide DeflectionOptics Foil cooling flakes STM Aluminium_Oxide Fluoride Metal-organicComplex Mechinical Electrical&Electronics Mechanical&nanotechnology Electronics Silicon LiftHeight LDPE Blend Inorganic_Compound polyvinyl acetate hetero_structure ForceVolumeMapping ContactMode PECurve ContactModeDots Sapphire conductive NtuEee Floppy Piezoelectric Polyvinylidene DeoxyribonucleicAcid ScanningThermalMicroscopy PolymerPatterns
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Carbon Nanotube on Si
Scanning Conditions
- System: XE7
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128