LaAlO3 Reduction AlkaneFilm Nanofiber NCM OxideLayer Writing non_contact Potential MechanicalProperties Gallium_Arsenide Plug KAIST TemperatureControlledAFM suspended_graphene Insulator Metal DiffractiveOpticalElements PolyvinylAcetate PolymerPatterns ForceVolumeImage FM-KPFM CeramicCapacitor FAPbI3 HDD Implant hetero_structure SicMosfet Film Chungnam_National_University LogAmplifier CarbonNanotube Techcomp CrAu hydrocarbon
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer Ι
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512