piezoelectric force microscopy Sic ScanningKelvinProbeMicroscopy InLiquid Calcite Chungnam_National_University ImideMonomer Annealing HexagonalBN ferromagnetic MagneticForce Fendb ring shape Microchannel Butterfly SSRM thermoplastic_elastomers phase_change exfoliate ThermalProperties mechanical_property ConductiveAFM ReflexLens gallium_nitride InorganicCompound atomic_layer Lattice Ram dichalcogenide Layer TPU Solution KelvinProbeForceMicroscopy Neodymium Photovoltaics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard disk media
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.250μm×0.250μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.250μm×0.250μm
- Scan Rate: 0.5Hz
- Pixel: 512×512