ScanningTunnelingMicroscopy ConductingPolymer CompactDisk UnivOfMaryland PVAC PhthalocyaninePraseodymium MolybdenumDisulfide LiftMode Chemical_Vapor_Deposition BlockCopolymer DentalProsthesis Galfenol CrossSection InLiquid StrontiumTitanate Sphere Boundary MechanicalProperty CarbonNanotube SoftSample GaAs Self-assembledMonolayer Writing Sadowski CrAu Formamidinium_lead_iodide Celebration Aggregated_molecules OpticalModulator Al2O3 ULCA TemperatureControllerStage University_of_Regensburg flakes Magnetostrictive
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512