Wonseok 2dMaterials MoS2 DLaTGS Polydimethylsiloxane Multiferroic_materials doped PVA AM-KPFM neodymium_magnets pinpoint mode Steps PolyimideFilm nanobar Ucl Lift molecular_self_assembly Collagen Oxide NeodymiumMagnets BiVO4 Lanthanum_aluminate Carbon HexagonalBoronNitride P3HT AmplitudeModulation PrCurve Chungnam_National_University membrane 2d_materials BaTiO3 epitaxy Polytetrafluoroethylene PFM DomainSwitching
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256