suspended_graphene VinylAlcohol Hair Polyimide FM_SKPM TungstenDeposition BTO ito_film LiquidCrystal ConductiveAFM CopperFoil StyreneBeads nanobar Steps Patterns kelvin probe force microscopy Moire Bacterium block_copolymer Oxidation Multiferroic_materials Microchannel KPFM Metal-organicComplex LateralPFM I-VSpectroscopy molecular_beam PrCurve ConductingPolymer cooling Polyvinylidene_fluoride Spain AM_KPFM Alloy margarine
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyaniline (PANI)
Scanning Conditions
- System: XE7
- Scan Mode: Non-contact
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512