Polytetrafluoroethylene cannabinoid INSPParis SurfaceChange Cobalt-dopedIronOxide Tape CNT Sidewall C60H122 Monisha Composition Hydroxyapatite Chungnam_National_University Korea CeramicCapacitor AM-KPFM Holes HOPG Pyroelectric ScanningThermalMicroscopy AdhesionEnergy molecular_beam MolecularSelfAssembly NusEce CrossSection self_healing SiWafer FM-KPFM Ito blended polymers Microchannel TransitionMetal PetruPoni_Institute ContactModeDot MultiferroicMaterials
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CTa2B12H12 Nanosheet
Scanning Conditions
- System : XE7
- Scan Mode: Contact, LFM
- Scan Rate : 0.5 Hz
- Scan Size : 6.5μm×6.5μm
- Pixel Size : 256×256
- Cantilever : RTESPA-150 (k=5N/m, f=150kHz)