Polypropylene SKKU Aluminum Pvdf FM_KPFM Bio Nanopattern CeramicCapacitor Electrical&Electronics AnodizedAluminumOxide PVAP3HT PatternedSapphireSubstrat PinpointNanomechanicalMode LateralForceMicroscopy TemperatureControllerAFM SICM MeltingPoint BismuthFerrite PDMS StainlessSteel temp IndiumTinOxide Hafnia Electical&Electronics FrictionalForce pinpoint mode Defects fifber AdhesionForce Magnets #Materials Blend Heat #EC Wang
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)