LiNbO3 PinpointNanomechanicalMode StyreneBeads LifeScience IRDetector Aggregated_molecules Semiconductor Mechinical Indent Polytetrafluoroethylene cannabidiol MfmAmplitude TappingMode TemperatureControl TemperatureControlledAFM Fluoride Growth mechanical property MagneticForce Piranha AdhesionEnergy temperature controller AFM Defect Phthalocyanine Sapphire GlassTemp RedBloodCell BaTiO3 Piezoresponse thermal_property Hole DLaTGS YttriaStabilizedZirconia SingleCrystal Pattern
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Strainded MoS₂ on Si
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : 0.15Hz
- Scan Size : 50μm×13μm
- Pixel Size : 2048×1024
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)