SrTiO3 Display Photovoltaics FM_KPFM dielectric trench Bmp thermoplastic_elastomers FrequencyModulation 3-hexylthiophene DNA Sadowski Polydimethylsiloxane Electronics CrossSection Piranha BariumTitanate GlassTemp Pyroelectric Aggregated_molecules Polarization Croatia CaMnO3 Zagreb SingleCrystal PvdfBead Platinum Anneal RedBloodCell FrictionForce Writing Phosphide CntFilm ForceVolumeMapping contact PinpointNanomechanicalMode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cowpea chlorotic mottle viruses (CCMV)
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 3 Hz
- Scan Size : 150nm×150nnm
- Pixel Size : 512×512
- Cantilever : SCOUT 350 (k=42N/m, f=350kHz)