Ceramics Organic Boundary Scratch Roughness suspended_graphene amplitude_modulation MfmAmplitude ReflexLens WPlug SFAs cannabis TungstenDeposition temp_control SKKU TemperatureControllerAFM Hydroxyapatite KelvinProbeForceMicroscopy SingleLayer Mfm Dr.JurekSadowski silicon_carbide Vacuum GlassTemp VerticalPFM ScanningTunnelingMicroscopy ThermalConductivity ForceVolume BismuthVanadate Lift epitaxy Deposition Ferrite TyphimuriumBiofilm Step
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
GaN epi wafer
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.7 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)