Polyurethane ReflexLens HafniumDioxide hard_disk EFM Domain Biofilm CVD Nanotechnology MechanicalProperty GalliumPhosphide ConductingPolymer Sphere KAIST thermoplastic_elastomers ForceVolume Oxidation Crystal Nanostructure Glass Growing TempControl KevlarFiber BismuthFerrite Hydroxyapatite NeodymiumMagnets Ito CuSubstrate layers alkanes Lattice Magnetic self_assembly amplitude_modulation phase_change
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256