Conductive AFM Heating Materials thermal_conductivity PtfeMembrane Array Mechanical AM_SKPM PvdfBead MechanicalProperties hetero_structure HighAcpectRatio SrO Yttria_stabilized_Zirconia atomic_steps Piezo PVA neodymium_magnets DNA NUSNNI Film SrTiO3 Anneal Optoelectronic polymeric_arrays fifber Molybdenum_disulfide HighResolution NusEce cannabidiol LogAmplifier KelvinProbeForceMicroscopy LaAlO3 FM_KPFM BreastCancerCell
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Al2O3-doped CaMnO3
1% Al2O3-doped CaMnO3 on LaAlO3 (001) orientation substrate by pulsed laser deposition.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256