Aluminum 2-vinylpyridine small_scan LFM Biology ScanningThermalMicroscopy StrontiuTitanate Fe_film OxideLayer SmalScan PolymerBlend Piezo LogAmplifier Worcester_Polytechnic_Institute electrospinning PetruPoni SoftSample Hafnium_dioxide MagneticArray Cobalt PANI CastIron Sphere LaAlO3 Electrode lithography temperature_control Leakage BoronNitride ContactModeDot block_copolymer Magnets AIN Nanofiber CrAu
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256