heterojunctions Calcite DNA Mechinical PatternedSapphireSubstrat Conductivity PhthalocyaninePraseodymium Indent Korea NeodymiumMagnets Deposition Boron domain_switching IMT_Bucharest CompactDisk C60H122 Ram MultiLayerCeramicCapacitor piezoelectric force microscopy ito_film Moire hard_disk ScanningIon-ConductanceMicroscopy CeNSE_IISc light_emission Silver UnivOfMaryland Piezoelectric Lateral_Force_Microscopy Switching Lanthanum_aluminate DIWafer Gong GaAs SmalScan
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Carbon Nanotube on Si
Scanning Conditions
- System: XE7
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128